Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 103 MPa @Strain 5.00 % |
14900 psi @Strain 5.00 % |
dry; ISO 604 |
Murtfeldt Murylat® Polyethylene Terephthalate Thanks to its extremely low absorption of moisture and low expansion coefficient, Murylat® is ideally suited for the processing of precision parts. Murylat® has an extremely high hardness grade an.. |