Mechanical Properties Metric English Comments
Compressive Yield Strength 100 MPa

@Strain 5.00 %
14500 psi

@Strain 5.00 %
dry; ISO 604
Murtfeldt Murylon® A Nylon 66
This material combines the excellent properties of the Murylon® range with additional high tensile and compressive strength, increased wear resistance, and a lower level of moisture absorption than..