Material Notes:
This material combines the excellent properties of the Murylon® range with additional high tensile and compressive strength, increased wear resistance, and a lower level of moisture absorption than Murylon® B.Special Properties:• High wear resistance• Improved tensile and compressive strength• High temperature resistance• Extremely good fatigue strength• Low cold flow characteristics• Approved for use in the food industry (EU and FDAInformation provided by Murtfeldt Kunststoffe GmbH & Co. KG.
Physical Properties Metric English Comments
Density 1.14 g/cc
0.0412 lb/in³
ISO 1183-1
Moisture Absorption at Equilibrium 2.4 %

@Temperature 23.0 °C
2.4 %

@Temperature 73.4 °F
50% RH
Water Absorption at Saturation 8.0 %

@Temperature 23.0 °C
8.0 %

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Rockwell M 88
88
dry; ISO 2039-2
Hardness, Shore D 81
81
DIN 53505
Ball Indentation Hardness 160 MPa
23200 psi
dry; ISO 2039-1
Tensile Strength, Yield 55.0 MPa
7980 psi
50% RH; ISO 527-1
90.0 MPa
13100 psi
dry; ISO 527-1
Elongation at Break 50 %
50 %
dry; ISO 527-1
>= 100 %
>= 100 %
50% RH; ISO 527-1
Modulus of Elasticity 1.70 GPa
247 ksi
50% RH
3.55 GPa
515 ksi
dry
Compressive Yield Strength 32.0 MPa

@Strain 1.00 %
4640 psi

@Strain 1.00 %
dry; ISO 604
62.0 MPa

@Strain 2.00 %
8990 psi

@Strain 2.00 %
dry; ISO 604
100 MPa

@Strain 5.00 %
14500 psi

@Strain 5.00 %
dry; ISO 604
Charpy Impact Unnotched NB
NB
dry; ISO 179-1/1eU
NB
NB
ISO 179
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
dry; ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.30
0.30
Sand Slurry 0.10
0.10
µm/km
Thermal Properties Metric English Comments
CTE, linear 80.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
44.4 µin/in-°F

@Temperature 73.4 - 140 °F
95.0 µm/m-°C

@Temperature 23.0 - 100 °C
52.8 µin/in-°F

@Temperature 73.4 - 212 °F
Thermal Conductivity 0.280 W/m-K
1.94 BTU-in/hr-ft²-°F
Melting Point 260 °C
500 °F
ISO 11357-1
Maximum Service Temperature, Air 80.0 °C

@Time 7.20e+7 sec
176 °F

@Time 20000 hour
95.0 °C

@Time 1.80e+7 sec
203 °F

@Time 5000 hour
180 °C

@Time <=86400 sec
356 °F

@Time <=24.0 hour
Minimum Service Temperature, Air -30.0 °C
-22.0 °F
Glass Transition Temp, Tg 60.0 °C
140 °F
ISO 11357-1
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Electrical Resistivity >= 1.00e+12 ohm-cm
>= 1.00e+12 ohm-cm
50% RH; IEC 60093
>= 1.00e+14 ohm-cm
>= 1.00e+14 ohm-cm
dry; IEC 60093
Surface Resistance >= 1.00e+12 ohm
>= 1.00e+12 ohm
50% RH; IEC 60093
>= 1.00e+13 ohm
>= 1.00e+13 ohm
dry; IEC 60093
Dielectric Constant 3.3

@Frequency 1.00e+6 Hz
3.3

@Frequency 1.00e+6 Hz
dry; IEC 60250
3.8

@Frequency 100 Hz
3.8

@Frequency 100 Hz
dry; IEC 60250
3.8

@Frequency 1.00e+6 Hz
3.8

@Frequency 1.00e+6 Hz
50% RH; IEC 60250
7.4

@Frequency 100 Hz
7.4

@Frequency 100 Hz
50% RH; IEC 60250
Dielectric Strength 18.0 kV/mm
457 kV/in
50% RH; IEC 60243-1
27.0 kV/mm
686 kV/in
dry; IEC 60243-1
Dielectric Loss Index 0.013

@Frequency 100 Hz
0.013

@Frequency 100 Hz
dry; IEC 60250
0.020

@Frequency 1.00e+6 Hz
0.020

@Frequency 1.00e+6 Hz
dry; IEC 60250
0.060

@Frequency 1.00e+6 Hz
0.060

@Frequency 1.00e+6 Hz
50% RH; IEC 60250
0.13

@Frequency 100 Hz
0.13

@Frequency 100 Hz
50% RH; IEC 60250
Compliance Properties Metric English Comments
European Food 1935/2004 Yes
Yes
FDA Yes
Yes
Descriptive Properties Value Comments
Color Natural/Black