Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.102 MPa @Strain 40.0 % |
14.8 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Compressive Yield Strength | 0.102 MPa @Strain 40.0 % |
14.8 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® LD33FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Compressive Yield Strength | 0.102 MPa @Strain 40.0 % |
14.8 psi @Strain 40.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® MP33 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |