Polymer Property : Compressive Yield Strength = 14.5 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 0.100 MPa

@Strain 50.0 %
14.5 psi

@Strain 50.0 %
BS ISO 7214 1998
Zotefoams Evazote® VA25 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Compressive Yield Strength 0.100 MPa

@Strain 50.0 %
14.5 psi

@Strain 50.0 %
ASTM 1056/85
Eurofoam Porocell POR 304 CM-KPA 45 EPDM Foam
Ethylene Propylene Diene Monomer Foam. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurofoam s.r.l.