Mechanical Properties Metric English Comments
Compressive Yield Strength 1234 MPa

@Temperature 71.0 °C
179000 psi

@Temperature 160 °F
Wet
Hexcel® HexPly® F593 Epoxy Resin, T2G190 Carbon Tape
Hexcel designation: T2GXXX-12"-F593; Fiber: Amoco T-300/12kInformation provided by HexCel
Compressive Yield Strength 1234 MPa

@Temperature 23.0 °C
179000 psi

@Temperature 73.4 °F
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Tape Form
Fiber: IM7-12KInformation provided by HexCel