Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.158 MPa @Strain 25.0 % |
22.9 psi @Strain 25.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® HD30 High Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Compressive Yield Strength | 0.158 MPa @Strain 25.0 % |
22.9 psi @Strain 25.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® LD70 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |