Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Yield Strength | 0.139 MPa @Strain 25.0 % |
20.2 psi @Strain 25.0 % |
BS ISO 7214 1998 |
Zotefoams Plastazote® LD50CN Conductive Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |