Mechanical Properties Metric English Comments
Compressive Yield Strength 0.0510 MPa

@Strain 25.0 %
7.40 psi

@Strain 25.0 %
BS ISO 7214 1998
Zotefoams Evazote® EV50 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Compressive Yield Strength 0.0510 MPa

@Strain 25.0 %
7.40 psi

@Strain 25.0 %
BS ISO 7214 1998
Zotefoams Evazote® VA35 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Compressive Yield Strength 0.0510 MPa

@Strain 25.0 %
7.40 psi

@Strain 25.0 %
BS ISO 7214 1998
Zotefoams Plastazote® LD24FR Low Density Polyethylene Foam, Flame Retardant
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Compressive Yield Strength 0.0510 MPa

@Strain 10.0 %
7.40 psi

@Strain 10.0 %
BS ISO 7214 1998
Zotefoams Plastazote® LD33 Low Density Polyethylene Foam
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Compressive Yield Strength 0.0510 MPa

@Strain 10.0 %
7.40 psi

@Strain 10.0 %
BS ISO 7214 1998
Zotefoams Plastazote® LD33FM Low Density Polyethylene Foam, Flame Retarded
Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs..
Compressive Yield Strength 0.0510 MPa

@Strain 40.0 %
7.40 psi

@Strain 40.0 %
BS ISO 7214 1998
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam
Supazote® is a closed cell, cross-linked copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstandi..
Compressive Yield Strength 0.0510 MPa

@Strain 25.0 %
7.40 psi

@Strain 25.0 %
ASTM 1056/85
Eurofoam Porocell POR 302/T-E NBR/PVC Foam
Acrylonitrile butadiene and polyvinyl chloride foam rubber. Used for thermal insulation and soundproofing, antivibration and waterproofing; different types of gaskets.Information provided by Eurof..