Mechanical Properties Metric English Comments
Ball Indentation Hardness 83.0 MPa
12000 psi
ISO 2039-1
Styrolution PS 576H HIPS
Styrolution PS 576H is a high gloss, high impact polystyrene with a good flow and good heat resistance.High gloss HIPSGood flow and heat resistanceHIPS with good balance of mechanical properties and..
Ball Indentation Hardness 83.0 MPa
12000 psi
358 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 500 HI4 POM
Easy flow high impact grade, possessing also high damping capacityInformation provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.