Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 72.0 MPa | 10400 psi | 132 N/10s; ISO 2039 |
Borealis HK030U Polypropylene Compound HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit.. |