Polymer Property : Ball Indentation Hardness = 10400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Ball Indentation Hardness 72.0 MPa
10400 psi
132 N/10s; ISO 2039
Borealis HK030U Polypropylene Compound
HK030U is a special low viscosity polypropylene compound developed to fit the production of PP-GF composites in the direct LFT compression and injection molding process as well as in combination wit..