Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 53.0 MPa | 7690 psi | ISO 2039-1 |
Azoty Tarnow™ TARFLEN SM-G20 PTFE Reinforced with 20% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |