Material Notes:
Reinforced with 20% graphite for standard compression molding.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A.
Physical Properties Metric English Comments
Density 2.16 g/cc
0.0780 lb/in³
ISO 1183
Filler Content 20 %
20 %
Graphite
Particle Size 40 µm
40 µm
Average
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ISO 868
Ball Indentation Hardness 53.0 MPa
7690 psi
ISO 2039-1
Tensile Strength, Yield 13.0 MPa
1890 psi
ISO 527
Elongation at Break 140 %
140 %
ISO 527
Izod Impact, Notched 2.00 J/cm
3.75 ft-lb/in
ISO 180
Thermal Properties Metric English Comments
CTE, linear 65.0 µm/m-°C

@Temperature 20.0 °C
36.1 µin/in-°F

@Temperature 68.0 °F
ASTM E 831
Melting Point 327 °C
621 °F
Flammability, UL94 V-0
V-0
Processing Properties Metric English Comments
Processing Temperature 370 °C
698 °F
Molding
Back Pressure 40.0 - 60.0 MPa
5800 - 8700 psi
Molding Pressure