Mechanical Properties Metric English Comments
Ball Indentation Hardness 270 - 360 MPa
39200 - 52200 psi
Average value: 320 MPa Grade Count:11
Overview of materials for Polyphthalamide (PPA)
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide". Each property range of values reported is minimum and maximum values of appropriate Ma..
Ball Indentation Hardness 340 - 360 MPa
49300 - 52200 psi
Average value: 353 MPa Grade Count:3
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..