Mechanical Properties Metric English Comments
Ball Indentation Hardness 340 - 360 MPa
49300 - 52200 psi
Average value: 353 MPa Grade Count:3
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi..
Ball Indentation Hardness 340 MPa
49300 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50
Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I...
Ball Indentation Hardness 340 MPa
49300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HTV-5H1 black 9205 PA6T/6I-GF50
Product description: Grivory HTV-5H1 black 9205 is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I...
Ball Indentation Hardness 340 MPa
49300 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSGL-60/4 black 9839 PA666-GF60
Product description: Grilon TSGL-60/4 black 9839 is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 black 9839 is characterized by the foll..
Ball Indentation Hardness 340 MPa
49300 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSGL-60/4 nat PA666-GF60
Product description: Grilon TSGL-60/4 natural is based on a heat stabilized semi-crystalline Polyamide PA66+PA6 and 60% long glass fibers. Grilon TSGL-60/4 natural is characterized by the following ..
Ball Indentation Hardness 340 MPa
49300 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50
Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
Ball Indentation Hardness 340 MPa
49300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT1V-5 FWA black 9225 PA6T/6I-GF50
Product description: Grivory HT1V-5 FWA black 9225 is a 50 wt.- % glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: ..
Ball Indentation Hardness 340 MPa
49300 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50
Product description: Grivory HT1V-5 FWA natural is a 50 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6..
Ball Indentation Hardness 340 MPa
49300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT1V-5 FWA nat PA6T/6I-GF50
Product description: Grivory HT1V-5 FWA natural is a 50 wt.-% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6..
Ball Indentation Hardness 340 MPa
49300 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50
Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl..
Ball Indentation Hardness 340 MPa
49300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HT1V-5 HY black 9205 PA6T/6I-GF50
Product description: Grivory HT1V-5 HY black 9205 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Grivory HT1V-5 HY bl..
Ball Indentation Hardness 340 MPa
49300 psi
dry; ISO 2039-1
EMS-Grivory Grivory® HTV-5H1 nat PA6T/6I-GF50
Product description: Grivory HTV-5H1 natural is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac..
Ball Indentation Hardness 340 MPa
49300 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® HTV-5H1 nat PA6T/6I-GF50
Product description: Grivory HTV-5H1 natural is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac..
Ball Indentation Hardness 340 MPa
49300 psi
ISO 2039-1
Akro-Plastic Akromid® T1 GF 50 9 (3257) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..