Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 32.0 MPa | 4640 psi | ISO 2039-1 |
Quadrant EPP TIVAR® Dryslide PE-UHMW + internal lubricant + other additives (ISO Data) Thanks to the lubricant built into a PE-UHMW matrix with higher molecular weight, TIVAR DrySlide offers a lower coefficient of friction and enhanced wear and abrasion resistance than TIVAR 1000. The.. |
|||
Ball Indentation Hardness | 32.0 MPa | 4640 psi | ISO 2039-1 |
Quadrant EPP TIVAR® TECH PE-UHMW + MoS2 (ISO Data) This PE-UHMW grade with extremely high degree of polymerisation contains molybdenum disulphide, resulting in a material with improved wear resistance and sliding properties over TIVAR 1000. |
|||
Ball Indentation Hardness | 32.0 MPa | 4640 psi | ASTM 1457-62 T |
Fluorseals PTFE 15% graphite filled Improved thermal conductivity and coefficient of friction.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Ball Indentation Hardness | 32.0 MPa | 4640 psi | DIN 2039 |
Wolf Kunststoff ZEDEX® ZX-550PV A7A Polymer Alloy Main Characteristics: Modified friction wear; Tough; Soft; Reduced wear at temperatures at 100 ° CApplications: Chemical Engineering; Laboratory Technology; Automitve Technology; Machine ToolsInfor.. |
|||
Ball Indentation Hardness | 32.0 MPa | 4640 psi | H 358/30; ISO 2039 |
Borealis Daplen™ EF261AI Polypropylene TPO Compound Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |