Material Notes:
Improved thermal conductivity and coefficient of friction.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials.
Physical Properties Metric English Comments
Density 2.17 g/cc
0.0784 lb/in³
ASTM 1457-62 T
Deformation 7.0 %
7.0 %
14 MPa, 100 h, 23°C; ASTM D621-59
Mechanical Properties Metric English Comments
Ball Indentation Hardness 32.0 MPa
4640 psi
ASTM 1457-62 T
Tensile Strength at Break 14.0 MPa
2030 psi
ASTM 1457-62 T
Elongation at Break 160 %
160 %
ASTM 1457-62 T
Coefficient of Friction, Dynamic 0.18 - 0.22
0.18 - 0.22
v = 1 m/s
0.20 - 0.23
0.20 - 0.23
v = 1.9 m/s
Abrasion 4.0
4.0
mm of depth after 70 hrs load duration; Partner Material ST 50
Thermal Properties Metric English Comments
CTE, linear 110 µm/m-°C

@Temperature 100 °C
61.1 µin/in-°F

@Temperature 212 °F
DIN 52328
Thermal Conductivity 0.930 W/m-K
6.45 BTU-in/hr-ft²-°F
DIN 52612
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+11 ohm-cm
1.00e+11 ohm-cm
DIN 53482
Surface Resistance 1.00e+12 ohm
1.00e+12 ohm
DIN 53482