Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 255 MPa | 37000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40 Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-4 FWA nat PA*-GF40 Product description: Grivory GV-4 FWA natural is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50 Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GV-5H black PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50 Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50 Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GV-5H PA*-GF50 Product description: Grivory GV-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GVL-4H nat PA*-GF40 Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GVS-5H nat PA*-GF50 Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSG-30/4 V0 PA666-GF30 FR Product description: Grilon TSG-30/4 V0 is a heat stabilized, flame retardant, self-extinguishing engineering thermoplastic, reinforced with glass-fiber 30% (by weight) based on a semi-crystalline P.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30 Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30 Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-4H PA*-GF40 Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide... |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50 Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam.. |
|||
Ball Indentation Hardness | 255 MPa @Load 36.5 kg |
37000 psi @Load 80.5 lb |
ISO 2039-1 |
Azoty Tarnow™ Tarnamid® T-27 CF30 Polyamide 6 30% Carbon Fiber - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | H 961/3000; ISO 2039-1 |
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GV-4H black PA*-GF40 Product description: Grivory GV-4H black 9915 is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |
|||
Ball Indentation Hardness | 255 MPa | 37000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50 Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami.. |