Mechanical Properties Metric English Comments
Ball Indentation Hardness 255 MPa
37000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GV-4 FWA black 9225 PA*-GF40
Product description: Grivory GV-4 FWA black 9225 is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copol..
Ball Indentation Hardness 255 MPa
37000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GV-4 FWA nat PA*-GF40
Product description: Grivory GV-4 FWA natural is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam..
Ball Indentation Hardness 255 MPa
37000 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GV-5 FWA black 9225 PA*-GF50
Product description: Grivory GV-5 FWA black 9225 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copoly..
Ball Indentation Hardness 255 MPa
37000 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GV-5H black PA*-GF50
Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Ball Indentation Hardness 255 MPa
37000 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GV-5H EF black 9915 PA*-GF50
Product description: Grivory GV-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Ball Indentation Hardness 255 MPa
37000 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GV-5H EF nat PA*-GF50
Product description: Grivory GV-5H EF natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyam..
Ball Indentation Hardness 255 MPa
37000 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GV-5H PA*-GF50
Product description: Grivory GV-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide..
Ball Indentation Hardness 255 MPa
37000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GVL-4H nat PA*-GF40
Product description: Grivory GVL-4H black is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 40% long glass fibers. Grivory GVL-4H blac..
Ball Indentation Hardness 255 MPa
37000 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GVS-5H nat PA*-GF50
Product description: Grivory GVS-5H natural is a 50% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyamide..
Ball Indentation Hardness 255 MPa
37000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® TSG-30/4 V0 PA666-GF30 FR
Product description: Grilon TSG-30/4 V0 is a heat stabilized, flame retardant, self-extinguishing engineering thermoplastic, reinforced with glass-fiber 30% (by weight) based on a semi-crystalline P..
Ball Indentation Hardness 255 MPa
37000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30
Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya..
Ball Indentation Hardness 255 MPa
37000 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® XE 4120 black 9916 PA*-GF30
Product description: Grivory XE 4120 black 9916 is a 30% glass fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semi-crystalline, partially aromatic copolya..
Ball Indentation Hardness 255 MPa
37000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GV-4H PA*-GF40
Product description: Grivory GV-4H natural is a 40% glass-fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyamide...
Ball Indentation Hardness 255 MPa
37000 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GVS-5H black 9915 PA*-GF50
Product description: Grivory GVS-5H black 9915 is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline polyamide with partially aromatic copolyam..
Ball Indentation Hardness 255 MPa

@Load 36.5 kg
37000 psi

@Load 80.5 lb
ISO 2039-1
Azoty Tarnow™ Tarnamid® T-27 CF30 Polyamide 6 30% Carbon Fiber - Antistatic and Electroconductive
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn..
Ball Indentation Hardness 255 MPa
37000 psi
H 961/3000; ISO 2039-1
Akro-Plastic Akromid® A3 GF 35 (2421) PA 6.6 Dry, 35% Glass Filled
AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat..
Ball Indentation Hardness 255 MPa
37000 psi
dry; ISO 2039-1
EMS-Grivory Grivory® GV-4H black PA*-GF40
Product description: Grivory GV-4H black 9915 is a 40% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..
Ball Indentation Hardness 255 MPa
37000 psi
conditioned; ISO 2039-1
EMS-Grivory Grivory® GV-5 FWA nat PA*-GF50
Product description: Grivory GV-5 FWA natural is a 50% glass fiber reinforced engineering thermoplastic material based on a combination of semicrystalline Polyamide with partially aromatic copolyami..