Ball Indentation Hardness 211 MPa
30600 psi
358 N; ISO 2039-1
Azoty Tarnow™ TARNOFORM 300 GF2 GB2 POM
10% glass fiber/10% glass beads mix reinforced injection molding grade, suitable for applications where increased strength and stiffness is required with care of the surface quality.Information prov..