Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 16.0 MPa | 2320 psi | ISO 2039-1 |
Iran Petrochemical (PCC) 1922T Low Density Polyethylene LDPE 1922T - for injection molding with a balance between flow properties and mechanical propertiesApplications: toys, household articles, clamping lids.Information provided by Iran Petrochemical Co.. |