Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Ball Indentation Hardness | 145 MPa | 21000 psi | dry; ISO 2039-1 |
Murtfeldt Murlubric® Oil Modified Nylon 6 Murlubric® is a modified cast polyamide that mineral oil is integrated into during polymerization. As a result, the material has self lubricating properties and retains its excellent characteristi.. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | ISO 2039-1 |
Nilit FRIANYL A63 N-SG5 Nylon 6.6 for injection molding, 5% mineral filled Nylon 6.6 for injection molding, low viscosity.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | ISO 2039-1 |
Nilit FRIANYL B63 KG30 Nylon 6 for injection molding, 30% chalk filled Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | ISO 2039-1 |
Nilit FRIANYL B63 KV15 Nylon 6 for injection molding, 15% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | ISO 2039-1 |
Nilit RECONYL A H Recycled nylon 6.6 for injection molding Recycled nylon 6.6 for injection molding, heat stabilized (available only in black).Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | ISO 2039-1 |
Quadrant EPP Ertalon® LFX PA 6 + oil, cast (ISO Data) This internally lubricated cast nylon 6 is self-lubricating in the real meaning of the word. Ertalon LFX, especially developed for unlubricated, highly loaded and slow moving parts applications, yie.. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | ISO 2039-1 |
Quadrant EPP Nylatron® LFG PA 6 + oil, cast (ISO Data) Nylatron LFG (Lubricated Food Grade) is self-lubricating in the real meaning of the word, and has a FDA food contact compliant composition. The Nylatron LFG has been specially developed for non-lubr.. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | ISO 2039-1 |
Nilit FRIANYL A63 BR80 Nylon 6.6 for injection molding, 80% bronze filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | ISO 2039-1 |
Nilit FRIANYL A63 HH Nylon 6.6 for injection molding Nylon 6.6 for injection molding, heat and hydrolysis stabilizedInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | ISO 2039-1 |
Nilit FRIANYL A63 V2 Nylon 6.6 for injection molding Nylon 6.6 for injection molding, flame retardant, free of halogen and phosphorus.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Ball Indentation Hardness | 145 - 220 MPa | 21000 - 31900 psi | Average value: 180 MPa Grade Count:6 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® AG-35 PA66-GF35 Product description: Grilon AG-35 is a heat stabilized, normal viscosity PA 66 injection molding grade with 35% glass fibers. High stiffnessHigh tensile strengthHigh heat distortion temperatureEasy .. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® EBV-15H black 9697 PA6-GF15 Product description: Grilon EBV-15H black 9697 is a high viscosity, heat stabilized PA6 extrusion blow molding grade with 15% glass fibers. Grilon EBV-15H black 9697 has the following important prop.. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® GTR 45 PA6I/6T Product description: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides.. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® GTR 45 PA6I/6T Product description: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides.. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | dry; ISO 2039-1 |
EMS-Grivory Grivory® TSS/4 PA666 Product description: Grilon TSS/4 is an unreinforced, heat stabilized, normal viscosity PA66 + PA6 injection molding grade. Grilon TSS/4 has the following important properties: Good flow behaviorEas.. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4106 black 9992 PA612-GF30 Product description: Grilamid XE 4106 black 9992 is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorpti.. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | conditioned; ISO 2039-1 |
EMS-Grivory Grivory® XE 4106 nat PA612-GF30 Product description: Grilamid XE 4106 natural is a 30% glass fiber reinforced, heat stabilized polyamide 612 injection molding grade. The main features of Grilamid XE 4106 are: low water absorptiong.. |
|||
Ball Indentation Hardness | 145 MPa @Time 30.0 sec |
21000 psi @Time 0.00833 hour |
DIN 53 456 |
Hippe PET Polyethylene Terephthalate Linear, saturated polyesters are thermoplastics which are used where good dimensional accuracy, high creep resistance and good sliding and wear behavior are required. Partially crystallized PET pos.. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | IEC 2039 |
BASF Ultraform N 2310P Q600 POM Ultraform N2310P Q600 is a general-purpose injection molding POM grade containing special lubricant. Low frictional coefficient giving extremely low wear with otherwise unaltered mechanical propert.. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | 358/30; ISO 2039-1 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | 358/30; ISO 2039 |
BASF Ultraform S 2320 003 UNC Q600 POM Ultraform S2320 003 UNC Q600 is an easy flowing and rapidly freezing injection molding POM grade. Contains a mold release agent. |
|||
Ball Indentation Hardness | 145 MPa @Load 36.5 kg, Time 30.0 sec |
21000 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® N2720 M210 POM Description: Is a POM, product with increased stiffness and strength as well as good wear characteristics, used, for instance, for sliding chains and conveyor systems.Information provided by BASF |
|||
Ball Indentation Hardness | 145 MPa @Load 36.5 kg, Time 30.0 sec |
21000 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® W2320 003 PRO POM Description: Is a POM, is a very easy flowing grade for thin-walled components with long flow paths.Information provided by BASF |
|||
Ball Indentation Hardness | 145 MPa @Load 36.5 kg, Time 30.0 sec |
21000 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® W2320 U03 POM Description: Very free-flowing, rapidly solidifying grade with UV stabilization for use where processing is extremely difficult but mechanical requirements are lower.Information provided by BASF |
|||
Ball Indentation Hardness | 145 MPa | 21000 psi | ISO 2039-1 |
BASF Ultraform W 2320 003 UNC Q600 POM Ultraform W2320 003 UNC Q600 is a very easy flowing and rapidly solidifying injection molding POM grade for use where processing is extremely difficult but mechanical properties are lower. Contains .. |
|||
Ball Indentation Hardness | 145 MPa @Load 36.5 kg, Time 30.0 sec |
21000 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® S2320 003 POM Description: Easy flowing and rapidly freezing grade for injection molding difficult, thin-walled part.Information provided by BASF |
|||
Ball Indentation Hardness | 145 MPa @Load 36.5 kg, Time 30.0 sec |
21000 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® S2320 003 PRO BK 00120 POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |
|||
Ball Indentation Hardness | 145 MPa @Load 36.5 kg, Time 30.0 sec |
21000 psi @Load 80.5 lb, Time 0.00833 hour |
ISO 2039-1 |
BASF Ultraform® S2320 003 PRO POM Description: Is a POM, is a standard flowing and rapidly freezing grade suitable for standard functional applications.Information provided by BASF |