Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Film Tensile Strength at Yield, TD | 24.0 MPa @Thickness 0.0200 mm |
3480 psi @Thickness 0.000787 in |
ISO 527-3 |
Total MDPE HR 515 Medium Density Polyethylene, Blown Film MDPE HR 515 is a medium density polyethylene produced with hexene as a co-monomer. It shows a broad molecular weight distribution ensuring outstanding processability.MDPE HR 515 is especially dedic.. |