Mechanical Properties Metric English Comments
Charpy Impact 12.2 J

@Tempering Temp. 538 °C
9.00 ft-lb

@Tempering Temp. 1000 °F
air cooled from 1900°F then tempered; V-notch
Crucible Steel WR-95 Tool Steel, AISI H10 Modified
WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight..
Charpy Impact 12.2 J

@Tempering Temp. 538 °C
9.00 ft-lb

@Tempering Temp. 1000 °F
air cooled from 1875°F then tempered; V-notch
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel
Crucible PDCQ™ is a premium version of H13, manufactured to exceed die casting industry specifications. PDCQ has at least 10 ft. lbs room temperature transverse toughness. Its enhanced toughness pr..
Charpy Impact 12.2 J

@Tempering Temp. 566 °C
9.00 ft-lb

@Tempering Temp. 1050 °F
air cooled from 1875°F then tempered; V-notch
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel
Crucible PDCQ™ is a premium version of H13, manufactured to exceed die casting industry specifications. PDCQ has at least 10 ft. lbs room temperature transverse toughness. Its enhanced toughness pr..