Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 71.9 J @Temperature 399 °C |
53.0 ft-lb @Temperature 750 °F |
Round bar 1" diameter, 310 HB |
EDRO #2 Prehardened 4130 Holder Block EDRO #2™ is a vacuum-degassed Chromium-Molybdenum-alloyed steel which is supplied in the hardened and tempered condition. EDRO #2™ is characterized by excellent machinability, good resistance to i.. |
|||
Charpy Impact | 71.9 J @Tempering Temp. 482 °C |
53.0 ft-lb @Tempering Temp. 900 °F |
hardened at 1475°F then tempered; C-notch |
Crucible Steel HALGRAPH® Tool Steel, AISI O6 Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a.. |