Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 31.2 J @Temperature -28.9 °C |
23.0 ft-lb @Temperature -20.0 °F |
|
Universal Wire Works 70S-6 Steel Welding Wire Universal 70S-6 is designed for welding mild steels with CO2 shielding gas. This alloy should be used where low silicon mild steel wires have not been satisfactory on slightly contaminated base meta.. |
|||
Charpy Impact | 31.2 J @Tempering Temp. 593 °C |
23.0 ft-lb @Tempering Temp. 1100 °F |
air cooled from 1850°F then tempered; V-notch |
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11 Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su.. |
|||
Charpy Impact | 31.2 J @Temperature 260 °C |
23.0 ft-lb @Temperature 500 °F |
38-40 HRC; V-notch |
Crucible Steel HALCOMB® 425 Tool Steel, AISI H19 Halcomb 425 is designed for higher operating temperatures than H13, where wear resistance and heat check resistance are more critical than toughness. While H19 has excellent heat checking resistance.. |