Mechanical Properties Metric English Comments
Charpy Impact 31.2 J

@Temperature -28.9 °C
23.0 ft-lb

@Temperature -20.0 °F
Universal Wire Works 70S-6 Steel Welding Wire
Universal 70S-6 is designed for welding mild steels with CO2 shielding gas. This alloy should be used where low silicon mild steel wires have not been satisfactory on slightly contaminated base meta..
Charpy Impact 31.2 J

@Tempering Temp. 593 °C
23.0 ft-lb

@Tempering Temp. 1100 °F
air cooled from 1850°F then tempered; V-notch
Crucible Steel HALCOMB® 218 Tool Steel, AISI H11
Halcomb 218 is a general purpose hot work tool steel, combining good toughness with moderate high-temperature strength and heat check resistance. Because of its high toughness, it is particularly su..
Charpy Impact 31.2 J

@Temperature 260 °C
23.0 ft-lb

@Temperature 500 °F
38-40 HRC; V-notch
Crucible Steel HALCOMB® 425 Tool Steel, AISI H19
Halcomb 425 is designed for higher operating temperatures than H13, where wear resistance and heat check resistance are more critical than toughness. While H19 has excellent heat checking resistance..