Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 27.1 J @Tempering Temp. 149 °C |
20.0 ft-lb @Tempering Temp. 300 °F |
hardened at 1475°F then tempered; C-notch |
Crucible Steel HALGRAPH® Tool Steel, AISI O6 Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a.. |
|||
Charpy Impact | 27.1 J @Tempering Temp. 260 °C |
20.0 ft-lb @Tempering Temp. 500 °F |
hardened at 1475°F then tempered; C-notch |
Crucible Steel HALGRAPH® Tool Steel, AISI O6 Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a.. |
|||
Charpy Impact | 27.1 J @Temperature 98.9 °C |
20.0 ft-lb @Temperature 210 °F |
V-notch (hardness of 45 HRC) |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |
|||
Charpy Impact | 27.1 J @Temperature 98.9 °C |
20.0 ft-lb @Temperature 210 °F |
V-notch (hardness of 45 HRC) |
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o.. |