Mechanical Properties Metric English Comments
Charpy Impact 27.1 J

@Tempering Temp. 149 °C
20.0 ft-lb

@Tempering Temp. 300 °F
hardened at 1475°F then tempered; C-notch
Crucible Steel HALGRAPH® Tool Steel, AISI O6
Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a..
Charpy Impact 27.1 J

@Tempering Temp. 260 °C
20.0 ft-lb

@Tempering Temp. 500 °F
hardened at 1475°F then tempered; C-notch
Crucible Steel HALGRAPH® Tool Steel, AISI O6
Halgraph is an oil-hardening graphitic tool steel with excellent non-deforming properties. Free graphite in its structure affords exceptional free-machining properties. The combination of graphite a..
Charpy Impact 27.1 J

@Temperature 98.9 °C
20.0 ft-lb

@Temperature 210 °F
V-notch (hardness of 45 HRC)
Bohler-Uddeholm UDDEHOLM ORVAR® SUPERIOR (Premium AISI H13) Hot Work Tool Steel
Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o..
Charpy Impact 27.1 J

@Temperature 98.9 °C
20.0 ft-lb

@Temperature 210 °F
V-notch (hardness of 45 HRC)
Bohler-Uddeholm UDDEHOLM ORVAR® SUPREME (Premium AISI H13) Hot Work Tool Steel
Chromium-molybdenum-vanadium alloyed steelA premium Cr-Mo-V-alloyed hot work die steel with good resistance to thermal fatigue. The steel is produced by a special melting and refining technique in o..