Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 16.3 J @Treatment Temp. 1070 °C |
12.0 ft-lb @Treatment Temp. 1950 °F |
hardened; C-notch |
Crucible Steel CSM® S60V (440V) Tool Steel, AISI 440C Modified CPM S60V is a unique tool steel made by the Crucible Particle Metallurgy process. It is designed from a 440C stainless base analysis with added high carbon and vanadium for exceptionally good wear r.. |
|||
Charpy Impact | 16.3 J @Temperature 260 °C |
12.0 ft-lb @Temperature 500 °F |
50 HRC; V-notch |
Crucible Steel PEERLESS A Tool Steel, AISI H21 Peerless A is designed for tools which will run hot, at operating temperatures between about 600F and 1100F. The tools should not be water cooled in service, due to a high risk of thermal shock. Pee.. |
|||
Charpy Impact | 16.3 J @Tempering Temp. 593 °C |
12.0 ft-lb @Tempering Temp. 1100 °F |
air cooled from 1900°F then tempered; V-notch |
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
Charpy Impact | 16.3 J @Temperature 399 °C |
12.0 ft-lb @Temperature 750 °F |
V-notch |
Bohler-Uddeholm UDDEHOLM HOTVAR® Hot Work Tool Steel Molybdenum-vanadium alloyed steelHotvar® is a premium hot work steel developed by Uddeholm to provide very good performance in tooling up to 1200°F (650°C). The alloying elements in Hotvar® are .. |