Mechanical Properties Metric English Comments
Charpy Impact 21.0 J

@Temperature -20.0 °C
15.5 ft-lb

@Temperature -4.00 °F
Transverse
ThyssenKrupp XABO® 355 Structural Steel
This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact 21.0 J

@Tempering Temp. 649 °C
15.5 ft-lb

@Tempering Temp. 1200 °F
air cooled from 1900°F then tempered; V-notch
Crucible Steel WR-95 Tool Steel, AISI H10 Modified
WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight..
Charpy Impact 21.0 J

@Temperature -20.0 °C
15.5 ft-lb

@Temperature -4.00 °F
Transverse
ThyssenKrupp XABO® 460 Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..