Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact | 19.0 J @Tempering Temp. 149 °C |
14.0 ft-lb @Tempering Temp. 300 °F |
hardened at 1475°F then tempered; C-notch |
Crucible Steel KETOS® Tool Steel, AISI O1 Ketos is an oil-hardening tool steel which may be hardened from fairly low temperatures with little size change. This grade combines deep-hardening qualities with a fine-grained structure, affording.. |
|||
Charpy Impact | 19.0 J @Tempering Temp. 621 °C |
14.0 ft-lb @Tempering Temp. 1150 °F |
air cooled from 1900°F then tempered; V-notch |
Crucible Steel WR-95 Tool Steel, AISI H10 Modified WR-95 is a modified H10, with cobalt added to improve its high temperature properties. It is an upgrade from H13 in applications requiring improved hot hardness or heat check resistance, at a slight.. |
|||
Charpy Impact | 19.0 J @Tempering Temp. 593 °C |
14.0 ft-lb @Tempering Temp. 1100 °F |
air cooled from 1875°F then tempered; V-notch |
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel Crucible PDCQ™ is a premium version of H13, manufactured to exceed die casting industry specifications. PDCQ has at least 10 ft. lbs room temperature transverse toughness. Its enhanced toughness pr.. |
|||
Charpy Impact | 19.0 J @Tempering Temp. 649 °C |
14.0 ft-lb @Tempering Temp. 1200 °F |
air cooled from 1875°F then tempered; V-notch |
Crucible Steel PDCQ Premium Quality High Toughness H13 Steel Crucible PDCQ™ is a premium version of H13, manufactured to exceed die casting industry specifications. PDCQ has at least 10 ft. lbs room temperature transverse toughness. Its enhanced toughness pr.. |