Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Stiffness = 120000 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Stiffness 827 MPa
120000 psi
ASTM D747
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..
Flexural Stiffness 827 MPa
120000 psi
ASTM D747
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..
Flexural Stiffness 827 MPa
120000 psi
ASTM D747
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..
Flexural Stiffness 827 MPa
120000 psi
ASTM D747
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..
Flexural Stiffness 827 MPa
120000 psi
ASTM D747
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..
Flexural Stiffness 827 MPa
120000 psi
ASTM D747
A. Schulman LP479-01 High-Density Polyethylene Homopolymer
DescriptionLP 479-01 is a high-density polyethylene homopolymer, offering good processability at high production rates. ApplicationUses of LP 479-01 include blown film and blow molded containers. In..