Mechanical Properties Metric English Comments
Flexural Stiffness 112.00 MPa
16244 psi
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane
Features: Excellent physical and low temperature properties with very good chemical resistance and wide processing window for extrusion.Uses: Flat die/cast film and tubing extrusion and Injection an..
Flexural Stiffness 112.00 MPa
16244 psi
ASTM D747
Lubrizol ESTANE® ETE50DS3 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Copyright © lookpolymers.com All Rights Reserved