Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 9.70 J | 7.15 ft-lb | ASTM D5420-93 |
Multibase Multi-Pro® 0110 X Natural Polypropylene This product is suitable for moldings incorporating high temperature requirements. This material is specially formulated to be resistant to Copper, but is also resistant to most metals.Data provide.. |