Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase Multi-Pro® 0110 X Natural Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Multibase
Trade Name Multi-Pro®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Pro® 0110 X Natural Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product is suitable for moldings incorporating high temperature requirements. This material is specially formulated to be resistant to Copper, but is also resistant to most metals.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.9055 g/cc
0.03271 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.018 - 0.022 cm/cm
0.018 - 0.022 in/in
ASTM D955-89
Melt Flow 4.0 g/10 min
4.0 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 33.8 MPa
4900 psi
ASTM D638-95
Elongation at Break 350 %
350 %
ASTM D638-95
Flexural Strength 37.2 MPa
5400 psi
ASTM D790-95
Flexural Modulus 1.414 GPa
205.1 ksi
Method 1, Proc. B; ASTM D-790-95
Izod Impact, Notched 0.370 J/cm
0.693 ft-lb/in
ASTM D256-93a
Gardner Impact 9.70 J
7.15 ft-lb
ASTM D5420-93
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved