Polymer Property : Gardner Impact = 5.65 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 5.65 J
4.17 ft-lb
ASTM D5420
RheTech Products RCC120-01 20% Calcium Carbonate Reinforced Polypropylene, Black, Recycled Content
Applications: Electrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 5.65 J
4.17 ft-lb
ASTM D5420
RheTech Products RCT220-01 20% Talc Reinforced Polypropylene Copolymer, Black, Recycled Content
Applications: Fan shroudsElectrical housingsHush panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 5.65 J
4.17 ft-lb
ASTM D5420
RheTech Products T20P250-00 20% Talc Reinforced Polypropylene Copolymer, Non-UV Stabilized, Natural
Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 5.65 J
4.17 ft-lb
ASTM D5420
RheTech Products T20P250-01 20% Talc Reinforced Polypropylene Copolymer, Black
Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 5.65 J
4.17 ft-lb
ASTM D5420
RheTech Products T20P250-01UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Black
Applications: Interior componentsI/P componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 5.65 J
4.17 ft-lb
ASTM D5420
RheTech Products T20P250-699UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AC20157-120 Black
Applications: Window trimCowl screensExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 5.65 J
4.17 ft-lb
ASTM D5420
RheTech Products T20P250-731UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AS20698 Black
Applications: Automotive trimIP componentsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 5.65 J
4.17 ft-lb
ASTM D5420
RheTech Products T30P200-01BG 30% Talc Reinforced Polypropylene Copolymer, Black, Blow Molding Grade
Applications: HVAC ductsSeat backsFlipper panelsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 5.65 - 36.2 J
4.17 - 26.7 ft-lb
Average value: 23.8 J Grade Count:17
Overview of materials for Polystyrene, Impact Modified
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a..
Gardner Impact 5.65 J

@Thickness 3.17 mm,
Temperature 23.0 °C
4.17 ft-lb

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D3029
Ineos Styrenics Avantra® 525K High Impact Styrenic Polymer (NAFTA)
Description: Specialty and super-high impact grades for a variety of applications such as refrigerator liners, consumer electronics housings, recreation equipment and sporting goods, toys, office pr..