Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 5.65 J | 4.17 ft-lb | ASTM D5420 |
RheTech Products RCC120-01 20% Calcium Carbonate Reinforced Polypropylene, Black, Recycled Content Applications: Electrical componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 5.65 J | 4.17 ft-lb | ASTM D5420 |
RheTech Products RCT220-01 20% Talc Reinforced Polypropylene Copolymer, Black, Recycled Content Applications: Fan shroudsElectrical housingsHush panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 5.65 J | 4.17 ft-lb | ASTM D5420 |
RheTech Products T20P250-00 20% Talc Reinforced Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 5.65 J | 4.17 ft-lb | ASTM D5420 |
RheTech Products T20P250-01 20% Talc Reinforced Polypropylene Copolymer, Black Applications: Air ductsHush panelsWire troughBracketsDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 5.65 J | 4.17 ft-lb | ASTM D5420 |
RheTech Products T20P250-01UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: Interior componentsI/P componentsInterior trimDurable goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 5.65 J | 4.17 ft-lb | ASTM D5420 |
RheTech Products T20P250-699UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AC20157-120 Black Applications: Window trimCowl screensExterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 5.65 J | 4.17 ft-lb | ASTM D5420 |
RheTech Products T20P250-731UV 20% Talc Reinforced Polypropylene Copolymer, UV Stabilized, AS20698 Black Applications: Automotive trimIP componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 5.65 J | 4.17 ft-lb | ASTM D5420 |
RheTech Products T30P200-01BG 30% Talc Reinforced Polypropylene Copolymer, Black, Blow Molding Grade Applications: HVAC ductsSeat backsFlipper panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 5.65 - 36.2 J | 4.17 - 26.7 ft-lb | Average value: 23.8 J Grade Count:17 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Gardner Impact | 5.65 J @Thickness 3.17 mm, Temperature 23.0 °C |
4.17 ft-lb @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D3029 |
Ineos Styrenics Avantra® 525K High Impact Styrenic Polymer (NAFTA) Description: Specialty and super-high impact grades for a variety of applications such as refrigerator liners, consumer electronics housings, recreation equipment and sporting goods, toys, office pr.. |