Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 6.78 J | 5.00 ft-lb | ASTM D5420 |
RheTech Products HP531-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Non-UV Stabilized, Natural Applications: IP structural componentsAir ducts - distributionA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 6.78 J | 5.00 ft-lb | ASTM D5420 |
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 6.78 J | 5.00 ft-lb | ASTM D5420 |
RheTech Products HP531-01UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: IP structural componentsAir ducts - distributionA/B/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 6.78 J | 5.00 ft-lb | ASTM D5420 |
RheTech Products HP531-678UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, IT3A Medium Light Stone Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 6.78 J | 5.00 ft-lb | ASTM D5420 |
RheTech Products HP531-679UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, 2B5A Black Ink Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 6.78 J @Temperature -29.0 °C |
5.00 ft-lb @Temperature -20.2 °F |
ASTM D3029 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Gardner Impact | 6.78 J | 5.00 ft-lb | ASTM D3029 |
Plastics Group Polifil® RMC-20 20% Calcium Carbonate-Reinforced Polypropylene, High Impact Polifil® RMC series compounds are high impact polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, they possess good stiffness, heat agin.. |
|||
Gardner Impact | 6.78 J | 5.00 ft-lb | ASTM D3029 |
Plastics Group Polifil® RMC-20V 20% Calcium Carbonate-Reinforced Polypropylene, High Impact, UV Stabilized Polifil® RMC-V series compounds are high impact, UV stabilized polypropylenes reinforced with fine particle size calcium carbonate. In addition to the highest impact possible, these compounds retar.. |
|||
Gardner Impact | 6.78 J @Temperature -29.0 °C |
5.00 ft-lb @Temperature -20.2 °F |
ASTM D3029 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Gardner Impact | 6.78 J @Temperature -29.0 °C |
5.00 ft-lb @Temperature -20.2 °F |
ASTM D3029 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Gardner Impact | 6.78 J @Temperature -29.0 °C |
5.00 ft-lb @Temperature -20.2 °F |
ASTM D3029 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Gardner Impact | 6.78 J @Temperature -29.0 °C |
5.00 ft-lb @Temperature -20.2 °F |
ASTM D3029 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Gardner Impact | 6.78 J @Temperature -29.0 °C |
5.00 ft-lb @Temperature -20.2 °F |
ASTM D3029 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Gardner Impact | 6.78 J | 5.00 ft-lb | ASTM D5420 |
RheTech Products CC20P100-01 20% Calcium Carbonate Reinforced Polypropylene, Black Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 6.78 J | 5.00 ft-lb | ASTM D5420 |
RheTech Products CC20P100-00 20% Calcium Carbonate Reinforced Polypropylene, Natural Applications: ElectronicsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |