Polymer Property : Gardner Impact = 4.51 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 4.51 J
3.33 ft-lb
ASTM D5420
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black
Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 4.51 J
3.33 ft-lb
ASTM D5420
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade
Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products.