Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 4.51 J | 3.33 ft-lb | ASTM D5420 |
RheTech Products FRP257-01 32% Talc Reinforced Polypropylene Copolymer, Flame Retardant, Black Applications: Electrical component housingsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 4.51 J | 3.33 ft-lb | ASTM D5420 |
RheTech Products GC8P200-00EG 8% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Natural, Extrusion Grade Applications: Extruded sheetWeather strippingInjection molding conditions reported in table.Information provided by RheTech Products. |