Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 30.4 J @Temperature -22.0 °C |
22.4 ft-lb @Temperature -7.60 °F |
Gardner |
Network Polymers NPP 25-0414 Description: Copolymer PolypropyleneInformation provided by Network Polymers Inc. |