Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Gardner Impact = 3.58 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 4.86 J

@Thickness 3.18 mm,
Temperature -23.0 °C
3.58 ft-lb

@Thickness 0.125 in,
Temperature -9.40 °F
ASTM D3029
PolyOne Maxxam™ PPC-40T Nat Polypropylene Copolymer (PP Copolymer)
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car..
Gardner Impact 4.86 - 4.86 J

@Temperature -23.0 - -23.0 °C
3.58 - 3.58 ft-lb

@Temperature -9.40 - -9.40 °F
Average value: 3.11 J Grade Count:1
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Gardner Impact 4.86 - 4.86 J

@Thickness 3.18 - 3.18 mm
3.58 - 3.58 ft-lb

@Thickness 0.125 - 0.125 in
Average value: 3.11 J Grade Count:1
Overview of materials for Polypropylene with 40% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are..
Gardner Impact 4.86 - 23.6 J

@Temperature -23.0 - -20.0 °C
3.58 - 17.4 ft-lb

@Temperature -9.40 - -4.00 °F
Average value: 19.8 J Grade Count:6
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..
Gardner Impact 4.86 - 23.6 J

@Thickness 3.17 - 3.18 mm
3.58 - 17.4 ft-lb

@Thickness 0.125 - 0.125 in
Average value: 19.8 J Grade Count:6
Overview of materials for Polypropylene Copolymer
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Copolymer". Each property range of values reported is minimum and maximum values of approp..
Copyright © lookpolymers.com All Rights Reserved