Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 24.3 J
17.9 ft-lb
ASTM D5420
RheTech Products HP534-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Natural
Applications: Door trim panelsCenter consolesSteering columnsInjection molding conditions reported in table.Information provided by RheTech Products.
Gardner Impact 24.3 J

@Temperature -30.0 °C
17.9 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Gardner Impact 24.3 J

@Temperature -30.0 °C
17.9 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Gardner Impact 24.3 J

@Temperature -30.0 °C
17.9 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Gardner Impact 24.3 J

@Temperature -30.0 °C
17.9 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Gardner Impact 24.3 J

@Temperature -30.0 °C
17.9 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..
Gardner Impact 24.3 J

@Temperature -30.0 °C
17.9 ft-lb

@Temperature -22.0 °F
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer
DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp..