Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 24.3 J | 17.9 ft-lb | ASTM D5420 |
RheTech Products HP534-00 22% Talc Reinforced High Performance Polypropylene Copolymer, Natural Applications: Door trim panelsCenter consolesSteering columnsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Gardner Impact | 24.3 J @Temperature -30.0 °C |
17.9 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Gardner Impact | 24.3 J @Temperature -30.0 °C |
17.9 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Gardner Impact | 24.3 J @Temperature -30.0 °C |
17.9 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Gardner Impact | 24.3 J @Temperature -30.0 °C |
17.9 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Gardner Impact | 24.3 J @Temperature -30.0 °C |
17.9 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |
|||
Gardner Impact | 24.3 J @Temperature -30.0 °C |
17.9 ft-lb @Temperature -22.0 °F |
|
A. Schulman POLYTROPE™ TPP 530 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 530 is an injection molding grade olefinic thermoplastic elastomer. This mineral filled product is recommended for applications requiring high stiffness and low thermal exp.. |