Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 28.5 J @Thickness 0.762 mm |
21.0 ft-lb @Thickness 0.0300 in |
ASTM D3029 |
SABIC Innovative Plastics Lexan® FR66 Polycarbonate Film, Flame Retardant Lexan FR66 flame-retardant film is a clear, thin-gauge polycarbonate film with a suede finish on one side and a matte finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Gardner Impact | 28.5 J @Thickness 0.762 mm |
21.0 ft-lb @Thickness 0.0300 in |
ASTM D3029 |
SABIC Innovative Plastics Lexan® FR83 Polycarbonate Film, Flame Retardant Lexan* FR83 flame-retardant film is a matt/polished, thin-gauge polycarbonate film with a UL94 VTM-0 listing to meet the stringent requirements in a wide range of electrical, electronic and transpor.. |
|||
Gardner Impact | 28.5 J @Thickness 0.762 mm |
21.0 ft-lb @Thickness 0.0300 in |
ASTM D3029 |
SABIC Innovative Plastics Lexan® FR60 Polycarbonate Film, Flame Retardant Lexan FR60 flame-retardant film is a clear, thin-gauge polycarbonate film with polished surfaces on both sides, and a UL94 V-0 listing to meet the stringent requirements in a wide range of electrica.. |
|||
Gardner Impact | 28.5 J @Thickness 0.762 mm |
21.0 ft-lb @Thickness 0.0300 in |
ASTM D3029 |
SABIC Innovative Plastics Lexan® FR63 Polycarbonate Film, Flame Retardant Lexan FR63 flame-retardant film is a clear, thin-gauge polycarbonate film with a matte finish on one side and a polish finish on the other and a UL94 V-0 listing to meet the stringent requirements i.. |
|||
Gardner Impact | 28.5 J @Temperature -29.0 °C |
21.0 ft-lb @Temperature -20.2 °F |
ASTM D5420G |
Braskem KN-501 Impact Copolymer Polypropylene Description: Excellent color and processing stability, excellent long term heat aging properties, wet / dry environment resistance.Applications: Suggested uses include automotive, housewares, toys, .. |
|||
Gardner Impact | 28.5 J | 21.0 ft-lb | ASTM D5420G |
Braskem TI4015F Impact Copolymer Polypropylene Description: Superior balance of stiffness and impact strength. Applications: Suggested uses include extrusion applications requiring good impact strength. Process: Extrusion. This resin meets the .. |
|||
Gardner Impact | 28.5 J | 21.0 ft-lb | ASTM D5420G |
Braskem TI4015F2 Impact Copolymer Polypropylene Description: Superior balance of stiffness and impact strength. Applications: Suggested uses include extrusion applications requiring good impact strength. Process: Extrusion. This resin meets the r.. |
|||
Gardner Impact | 28.5 J @Thickness 0.762 mm |
21.0 ft-lb @Thickness 0.0300 in |
ASTM D3029 |
SABIC Innovative Plastics Lexan® FR65 Polycarbonate Film, Flame Retardant Lexan FR65 flame-retardant film is a clear, thin-gauge polycarbonate film with a velvet finish on one side and a matt finish on the other, and a UL94 V-0 listing to meet the stringent requirements i.. |