Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 28.0 J @Temperature -40.0 °C |
20.7 ft-lb @Temperature -40.0 °F |
|
Shell Carilon® DP P1000 Polyketone
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON® Thermoplastic Polymer DP P1000 is the first in a family of developmental engineering polyketone resins fr.. |
|||
Gardner Impact | 28.0 J @Temperature -30.0 °C |
20.7 ft-lb @Temperature -22.0 °F |
ASTM D5420 |
Flint Hills AP4135-HS Polypropylene Impact Copolymer Features: Excellent processability, good low temperature impact strength.Applications: Injection Molding: Large, thin wall parts and house waresInformation Provided by Flint Hills Resources |
|||
Gardner Impact | 28.0 J @Temperature -30.0 °C |
20.7 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
Flint Hills AP6412-HS Impact Copolymer Polypropylene High impact copolymer, and FDA compliant. Features: Blush resistant and heat stabilized.Applications: Injection molding: consumer durables, automotive interior trim, furniture trim and housing, and .. |
|||
Gardner Impact | 28.0 J @Temperature 23.0 °C |
20.7 ft-lb @Temperature 73.4 °F |
ASTM D5420 |
Flint Hills P5M2Z-012 Polypropylene Random Copolymer Features: Good contact clarity. Product does not contain animal derived components. Phthalate-free.Applications: Extrusion: film and blow moldingInformation Provided by Flint Hills Resources |
|||
Gardner Impact | 28.0 J | 20.7 ft-lb | ASTM D3029 |
LyondellBasell Astryn BA45H Polypropylene Copolymer, Flame Retardant Key Features: medium melt flow, medium modulus, flame retardant polypropylene copolymer, UL 94 V-2 flames, good electrical properties and insulating characteristics, good aesthetics and colorability.. |
|||
Gardner Impact | 28.0 J @Temperature -30.0 °C |
20.7 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
LyondellBasell Hifaxâ„¢ ETA-3131E Thermoplastic Olefin Resin Key Features: fractional melt flow, medium modulus, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good practical impact, good processabilityApplications: molded.. |
|||
Gardner Impact | 28.0 J @Temperature -40.0 °C |
20.7 ft-lb @Temperature -40.0 °F |
|
Shell Carilon® D26HM100 Polyketone, General-Purpose Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26HM100 is a general-purpose injection molding grade with mechanical properties which classify it .. |
|||
Gardner Impact | 28.1 J | 20.7 ft-lb | CP-TM-11 |
PolyOne Elastamax HTE 2101-1000 Polyurethane Alloy
(discontinued **) This is an extrusion grade polyurethane alloy. Physical Form: Pellet. Standard Color: Off white, opaque.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000. .. |
|||
Gardner Impact | 28.0 J @Temperature -30.0 °C |
20.7 ft-lb @Temperature -22.0 °F |
ASTM D3029 |
LyondellBasell Hifax™ CB235 Thermoplastic Olefin Resin Key Features: medium high melt flow, medium high modulus, paintable thermoplastic olefin resin, excellent impact and stiffness balance, good dimensional stability, excellent processability, good pai.. |