Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Gardner Impact | 23.6 J @Thickness 3.17 mm, Temperature -28.9 °C |
17.4 ft-lb @Thickness 0.125 in, Temperature -20.0 °F |
Geometry GC; ASTM D5420 |
ExxonMobil PP9074MED Polypropylene Homopolymer Product Description: A highly clarified random copolymer resin designed for injection molding of medical devices suitable for sterilization by high energy radiation.Availability: Europe and North A.. |