Polymer Property : Gardner Impact = 17.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 23.0 J
17.0 ft-lb
ASTM D3029
SABIC Innovative Plastics ULTEM 1100 PEI
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing.
Gardner Impact 23.0 J
17.0 ft-lb
ASTM D3029
SABIC Innovative Plastics ULTEM 1100 PEI (Asia Pacific)
Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing.
Gardner Impact 23.0 J
17.0 ft-lb
ASTM D3029
SABIC Innovative Plastics ULTEM 1110 PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming.
Gardner Impact 23.0 J
17.0 ft-lb
ASTM D3029
SABIC Innovative Plastics ULTEM 1110 PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming.
Gardner Impact 23.0 J
17.0 ft-lb
ASTM D3029
SABIC Innovative Plastics ULTEM 1110F PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant, NSF 51 listing. UL94 V0 and 5VA listing. Effective June 2007, this grade will no longer be supported w..
Gardner Impact 23.0 J
17.0 ft-lb
ASTM D3029
SABIC Innovative Plastics ULTEM 1110F PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be supported wit..
Gardner Impact 23.0 J

@Temperature 23.0 °C
17.0 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Ultem 1110R PEI
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region.
Gardner Impact 23.0 J

@Temperature 23.0 °C
17.0 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region.
Gardner Impact 23.0 J

@Temperature 23.0 °C
17.0 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East)
Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Gardner Impact 23.0 J
17.0 ft-lb
ASTM D3029
SABIC Innovative Plastics ULTEM HU1110 PEI
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
Gardner Impact 23.0 J
17.0 ft-lb
ASTM D3029
SABIC Innovative Plastics ULTEM HU1110 PEI (Asia Pacific)
Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac..
Gardner Impact 23.0 J
17.0 ft-lb
ASTM D3029
SABIC Innovative Plastics ULTEM MD131A PEI
Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.
Gardner Impact 23.0 J

@Temperature 23.0 °C
17.0 ft-lb

@Temperature 73.4 °F
ASTM D 3029
SABIC Innovative Plastics Ultem MD131A PEI (Europe-Africa-Middle East)
Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.